Process optimization for hot forging of difficult parts by computer experiments and response surface analysis


Kabataş B., LİVATYALI H., AŞÇIOĞLU TEMİZTAŞ B.

Journal of Advances in Manufacturing Engineering, cilt.3, sa.2, ss.33-45, 2022 (Hakemli Dergi)