Chracterization of Creep Behavior of Epoxy and Graphene-Epoxy Nancomposite using Nanoindentation
Copy For Citation
ÇOLAK ÇAKIR Ö. Ü.
Multiphase Polymer and Polymer Composites, 01 June 2011
-
Publication Type:
Conference Paper / Full Text
-
Yıldız Technical University Affiliated: