Performance of LC3 mortars with cement contents below 50%: Effects of reactive MgO and red mud
Construction and Building Materials, cilt.550, 2026 (SCI-Expanded, Scopus)
- Yayın Türü: Makale / Tam Makale
- Cilt numarası: 550
- Basım Tarihi: 2026
- Doi Numarası: 10.1016/j.conbuildmat.2026.148849
- Dergi Adı: Construction and Building Materials
- Derginin Tarandığı İndeksler: Science Citation Index Expanded (SCI-EXPANDED), Scopus, Compendex, INSPEC
- Anahtar Kelimeler: Embodied carbon, Limestone calcined clay cement (LC3), Low-carbon cement, Reactive MgO, Red mud, Rheology
- Yıldız Teknik Üniversitesi Adresli: Evet
Özet
Further reduction in the cement content of limestone calcined clay cement (LC3) offers opportunities to lower embodied carbon, although maintaining satisfactory fresh-state and mechanical performance remains challenging. This study investigates reactive magnesium oxide (r-MgO) and uncalcined red mud (RM), individually and in combination, as additional cement-replacement constituents in LC3-based mortars incorporating waste marble dust as the carbonate source. Mixtures containing 40% and 30% cement were evaluated through flowability, setting time, rheology, semi-adiabatic calorimetry, X-ray diffraction, thermogravimetric analysis, physical water-loss measurements, mechanical properties, and drying shrinkage, alongside a material-stage embodied carbon assessment. At 40% cement, the incorporation of 10% r-MgO or RM resulted in 28-day compressive strengths of 46.7 and 46.5 MPa, respectively, exceeding both LC3 (43.8 MPa) and the reference mortar (40.1 MPa). Despite their comparable mechanical performance, r-MgO substantially increased rheological resistance and accelerated setting, whereas RM maintained more favorable workability. Further reduction in cement content to 30% revealed contrasting responses: 20MG exhibited poor workability and reduced compressive strength (26.4 MPa), while 20RM maintained 41.3 MPa. The combined incorporation of r-MgO and RM provided no clear synergistic benefit. Notably, 20RM achieved an estimated 61% reduction in material-stage embodied CO2 relative to the reference while retaining comparable compressive strength. These findings demonstrate that cement content can be reduced from 50% to 30% within the investigated LC3-based formulations through the incorporation of uncalcined RM, while retaining a 28-day compressive strength of 41.3 MPa and substantially reducing the estimated material-stage embodied carbon, highlighting its potential for developing lower-carbon construction materials.